Fused cast AZS block
Other name: Zircon-corundum brick
Model Number: AZS 33# PT, AZS 36 PT/WS, AZS 41# WS
Certification: ISO 9001-14001
Minimum Order Quantity: 5 MT
Fused cast AZS block
Description:
Fused cast AZS block is the most important refractory material for ensuring the normal operation of the glass melting furnace. At present, the glass melting furnace in the world increases the melting rate, prolongs the kiln age, and reduces the fuel consumption mainly because of the use of fused cast AZS block. Its performance increases as the ZrO2 content increases.
Advantages:
High refractoriness under load, high strength, good resistance to glass melt erosion, not polluting the glass melt
Application:
Glass melting furnace/kiln, side wall of the melting tank, superstructure, dog-hole corner, throat etc. ...
Casting process:

Fused cast AZS block physical and chemical
| Chemical Composition ( % ) | AZS 33 | AZS 36 | AZS 41 | |
| ZrO2 | ≥ 32.5 | ≥ 36 | ≥ 40.5 | |
| SiO2 | ≤ 15.5 | ≤ 14.0 | ≤ 12.5 | |
| Al2O3 | Remains | Remains | Remains | |
| Na2O | ≤ 1.4 | ≤ 1.6 | ≤ 1.2 | |
| Fe2O3 + TiO2 | ≤ 0.25 | ≤ 0.25 | ≤ 0.25 | |
| Physical characters | ||||
| Volume density (hardest part) | ≥ 3.80 | ≥ 3.85 | ≥ 4.05 | |
| Cold crushing strength (Mpa) | ≥ 300 | ≥ 300 | ≥ 300 | |
| Exudation Temp. of glass phase (℃) | ≥ 1400 | ≥ 1410 | ≥ 1420 | |
| Refractoriness under load (0.2MPa) | 1700 | 1700 | 1700 | |
| Corrosion Resistance to glass melt 1300℃ x10h (mm/24hr) | 1.4 | 1.3 | 1.2 | |
| Bulk density (g/cm3 ) | PT | ≥3.42 | ≥3.5 | ≥3.55 |
| QX | ≥3.45 | - | - | |
| ZWS | ≥3.65 | ≥3.65 | ≥3.85 | |
| WS | ≥3.7 | ≥ 3.75 | ≥3.95 | |
| Crystalline phase composition (%) | ||||
| Baddeleyite monocrystal | 32 | 35.5 | 40 | |
| Glass phase | 20 | 19 | 17 | |
| Corundum | 47 | 44 | 42 | |